On this mug made in ligt clay (208 Goerg & Schneider – Silicanordic), I have first glazed the inside with sand with effect ( Silicanordic 42008). Thereafter, the top of the outside is glazed twice with a brush glaze Travertin (Botz 9899), and when it is dried, the bottom is dipped in sand with effect.
It is fired to 1230 degrees.
This mug is glazed with the same glazes like the one above, but on this mug is the whole outside glazed twice with Travertin and the clay is 933 with cork spots, Goerg & Schneider altso from Silicanordic.